PEMANFAATAN LIMBAH PLASTIK SEBAGAI AGREGAT KASAR TERHADAP KUAT TEKAN BETON

Dharmawan, Rendy Arditya (2023) PEMANFAATAN LIMBAH PLASTIK SEBAGAI AGREGAT KASAR TERHADAP KUAT TEKAN BETON. Sarjana (S1) thesis, Universitas Islam 45 Bekasi.

[img] Text
Pendahuluan.pdf.pdf

Download (1MB)
[img] Text
BAB I.pdf
Restricted to Repository staff only

Download (121kB) | Request a copy
[img] Text
BAB II.pdf
Restricted to Repository staff only

Download (362kB) | Request a copy
[img] Text
BAB III.pdf
Restricted to Repository staff only

Download (441kB) | Request a copy
[img] Text
BAB IV.pdf
Restricted to Repository staff only

Download (854kB) | Request a copy
[img] Text
BAB V.pdf
Restricted to Repository staff only

Download (8kB) | Request a copy
[img] Text
DAFTAR PUSTAKA.pdf

Download (95kB)

Abstract

ABSTRAK Plastic has become the most popular object in everyday life. Many people are not aware of the dangers that will be caused by the use of plastic to health and to the surrounding environment. The use of plastic packaging which is very large, also has an impact on the environment because a lot of plastic is recommended for single use only. This has a negative impact on the environment, especially on the soil, because it is difficult for micro-organisms in the soil to decompose the plastic waste. The problem arises when we no longer need these things. There should be a way to process or utilize this used plastic waste. So the thought arose to utilize plastic waste to be used as artificial gravel for the compressive strength of concrete. In this study, the compressive strength analysis of concrete was carried out. The test object is a cylinder measuring 15 x 30 cm consisting of 4 variations, namely: normal cylinder and cylinder with a mixture of plastic waste (artificial gravel). The results show that the average compressive strength of concrete at 28 days is 19.415 MPa at 0% variation, 17.894 MPa at 3% variation, 16.526 MPa at 6% variation and 15.409 MPa at 9% variation. In the 3% addition variation of 17.894 MPa it is still included in the design compressive strength of 17.5 MPa, but in the following variations it has decreased.

Item Type: Thesis (TA, Skripsi, Tesis, Disertasi) (Sarjana (S1))
Contributors/Dosen Pembimbing,NIDN Dosen bisa diakses di LINK https://bit.ly/NIDNdosenunismabekasi:
ContributionContributors / Dosen PembimbingNIDN
UNSPECIFIEDNuryati, Sri0407126801
UNSPECIFIEDParyati, Ninik0429017903
Keywords / Kata Kunci: Kerikil tiruan, kuat tekan beton
Subjects: Struktur (Perancangan Gedung)
Faculty: Fakultas Teknik > Teknik Sipil S1
Depositing User: Mr Rendy Arditya
Date Deposited: 09 Nov 2023 02:54
Last Modified: 09 Nov 2023 03:24
URI: http://repository.unismabekasi.ac.id/id/eprint/4264